ASTM C657 D-C Volume Resistivity of Glass

ASTM C657 determines the D-C volume resistivity of a smooth, polished glass by measuring the resistance by passing a tiny amount of direct current through the glass. Assuring the grade of the glass, especially for the needs in the defense and aerospace industry.

    Talk to an Expert
    ASTM C657 D-C Volume Resistivity of Glass

    TRUSTED BY

    Precision-driven testing for dimensional accuracy and compliance

    • Overview
    • Scope, Applications, and Benefits
    • Test Process
    • Specifications
    • Instrumentation
    • Results and Deliverables

    Overview

    ASTM C657 prescribes the test procedure for determining the D-C volume resistivity of glass materials. The test method measures the resistance of glass to the flow of direct electric current through a definite unit volume under an applied voltage.

    This test method applies to service conditions in which glass is used as an electrical insulating material or is subjected to electric fields. ASTM C657 is designed to yield reliable data on the electrical resistivity of glass, enabling the assessment of insulation performance and safety for use in electrical, telecommunications, aerospace, and defense applications.

    Scope, Applications, and Benefits

    Scope

    ASTM C657 outlines procedures for measuring the electrical resistivity of glass using D-C (and A-C) methods under controlled environmental conditions.
    It evaluates:

    • D-C volume resistivity of glass materials
    • Electrical insulation capability under applied voltage
    • Influence of specimen geometry and test conditions on resistivity
    • Suitability of glass for electrical and electronic applications

    The method applies to flat glass specimens used in insulating and high-performance electrical environments.

    Applications

    • Electrical insulation components and systems
    • Telecommunications and optical fiber materials
    • Glass used in electronic and electrical manufacturing
    • Aerospace and defense electrical insulation applications
    • Research and development of specialized glass compositions
    • Quality control and material qualification testing

    Benefits

    • Provides a standardized method for determining electrical insulation properties
    • Ensures material compliance with safety and performance requirements
    • Supports material selection for electrical and electronic applications
    • Enables comparison of glass materials under identical test conditions
    • Improves confidence in product reliability and performance
    • Promotes innovation in advanced glass formulations

    Test Process

    Specimen Preparation

    Glass specimens are prepared as flat, defect-free plates to avoid influence on electrical measurements.

    1

    Test Environment Setup

    Testing is performed under controlled temperature and humidity conditions for accuracy and repeatability.

    2

    Electrode Placement & Electrical Measurement

    Electrodes are applied to the specimen, and a suitable D-C voltage is applied; the resulting current through the glass thickness is measured.

    3

    Resistivity Determination

    Volume resistivity is calculated using the measured current, applied voltage, and specimen dimensions.

    4

    Technical Specifications

    ParameterDetails
    Applicable MaterialsGlass materials used for electrical insulation
    Specimen GeometryFlat glass plates
    Thickness RangeApproximately 1 mm to 10 mm
    Cross-Sectional AreaTypically 10 cm² to 100 cm²
    Test EnvironmentControlled temperature and humidity
    Measured OutputsApplied voltage, current, volume resistivity
    Result UnitsOhm-centimeters (Ω·cm)

    Instrumentation Used for Testing

    • D-C power supply
    • Precision voltmeter
    • Precision ammeter
    • Electrode assemblies
    • Environmental control system (temperature and humidity)
    • Measuring tools for specimen dimensions
    • Data recording and calculation tools

    Results and Deliverables

    • D-C volume resistivity values of glass specimens (Ω·cm)
    • Electrical insulation performance assessment
    • Data supporting material qualification and quality control
    • Comparative resistivity data for different glass compositions
    • Documentation for safety, performance, and design validation

    Frequently Asked Questions

    ASTM C657 D-C is a standard test method for measuring the volume resistivity of glass.

    Volume resistivity is a critical property for assessing the suitability of glass in electrical applications.

    The volume resistivity of glass generally falls within the range of 10⁸ to 10¹⁶ ohm-centimeters (Ω·cm). Higher values indicate better insulating properties.

    The specimen used in ASTM C657 should possess a flat glass plate with a 1 mm to 10 mm thickness. The cross-sectional area should be large enough to properly contact the electrodes, and can be between 10 cm² and 100 cm².

    ASTM C657 is mainly designed for testing glass. Similar principles can be applied to measure the resistivity of other non-conductive materials. Still, they might require different standards or testing methods.

    Case Studies

    In-depth examination of genuine material testing solutions

    Dopant and Ultra-Low Concentration Elemental Analysis Using STEM…

    banner

    Dopant and Ultra-Low Concentration Elemental Analysis Using STEM…

    Introduction to STEM-EELS for Elemental Analysis Scanning Transmission Electron Microscopy (STEM) combined with Electron Energy Loss...

    Read Case Study

    Analysis of PVC Pipe Degradation Using FTIR Spectroscopy

    Fourier Transform Infrared Spectroscopy (FTIR)

    Analysis of PVC Pipe Degradation Using FTIR Spectroscopy

    PVC Pipe in Infrastructure — and Why Degradation Matters Polyvinyl chloride (PVC) pressure pipe is one...

    Read Case Study

    Nano-scale roughness measurement of Si-wafers by Atomic Force…

    banner

    Nano-scale roughness measurement of Si-wafers by Atomic Force…

    Nano-scale surface roughness is a critical parameter in fabricated thin-films that are used in optics, solar...

    Read Case Study
     Request a Quote

    Request a Quote

    Submit your material details and receive testing procedures, pricing, and turnaround time within 24 hours.



    • ddd
      Quick Turnaround and Hasslefree process
    • ddd
      Confidentiality Guarantee
    • ddd
      Free, No-obligation Consultation
    • ddd
      100% Customer Satisfaction
    Home / ASTM / ASTM C657 D-C Volume Resistivity of Glass

    Discover more from Infinita Lab

    Subscribe now to keep reading and get access to the full archive.

    Continue reading

    ×

    Talk to an Expert

      Connect Instantly

      (888) 878-3090
      Ensure Quality with the Widest Network of Accredited Labs
      • ddd
        Quick Turnaround and Hasslefree process
      • ddd
        Confidentiality Guarantee
      • ddd
        Free, No-obligation Consultation
      • ddd
        100% Customer Satisfaction

        ddd

        Start Material Testing