ASTM D2584 Ignition Loss of Cured Reinforced Resins

Ignition Loss Test of Cured Reinforced Resins by ASTM D2584 is done in cured reinforced resins to evaluate the fiber content remaining after burning. This helps in evaluating the composition of the test material. Read more about ASTM D2584 Ignition Loss of Cured Reinforced Resins below.

    Talk to an Expert
    Default Image

    TRUSTED BY

    Precision-driven testing for dimensional accuracy and compliance

    • Overview
    • Scope, Applications, and Benefits
    • Test Process
    • Specifications
    • Instrumentation
    • Results and Deliverables

    Overview

    ASTM D2584 is a test method that determines the amount of material left after a controlled burning of the cured reinforced resin. Weighing the residue left after ignition isolates the inorganic material, or glass fibers, in the sample.

    In a composite material that is a combination of glass reinforcement and organic resin, the ignition loss is a direct measure of the amount of resin in the material. This is a common method used to determine the ratio of fibers to resin in reinforced plastics.

    Scope, Applications, and Benefits

    Scope

    ASTM D2584 applies to cured reinforced resin systems, particularly glass fiber reinforced plastics (GFRP) and other thermoset composite materials. The standard outlines a test method for determining material composition by measuring weight loss after ignition, which helps quantify resin and fiber content in the composite.

    It determines:

    • Ignition loss percentage
    • Resin content (when only glass reinforcement is present)
    • Fiber content after burn-off

    Applications

    • Quality control of reinforced composites
    • Verification of fiber-resin ratio
    • Incoming inspection of composite laminates
    • Process validation in composite manufacturing
    • Marine composite products
    • Construction panels and structural composites
    • Research and development of reinforced resins

    Benefits

    • Simple and reliable determination of resin content
    • Accurate evaluation of fiber percentage
    • Supports process consistency
    • Improves composite material performance control
    • Ensures compliance with material specifications
    • Provides standardized and repeatable testing procedure

    Test Process

    Specimen Preparation

    Condition three ~5 g specimens for at least 40 hours at laboratory conditions. Prepare pre-weighed, pre-dried crucibles.

    1

    Initial Weighing

    Weigh each specimen to the nearest 0.1 mg and record the initial weight.

    2

    Ignition & Cooling

    Place specimens in crucibles and heat at 565°C ± 28°C until all ორგანics are burned off. Cool in a desiccator.

    3

    Final Weighing & Calculation

    Measure the residue weight and calculate ignition loss percentage from the weight difference.

    4

    Technical Specifications

    ParameterDetails
    Applicable MaterialsCured reinforced resins (typically glass fiber composites)
    Furnace Temperature565°C ± 28°C
    Specimen WeightApproximately 5 g
    Specimen DimensionsApprox. 2.5 in × 2.5 in × required thickness
    Number of SpecimensThree
    Measurement Accuracy0.1 mg (analytical balance)

    Instrumentation Used for Testing

    • Muffle furnace (capable of 565°C ± 28°C)
    • Ceramic or metal crucibles
    • Analytical balance (0.1 mg precision)
    • Desiccator
    • Conditioning chamber (standard laboratory atmosphere)
    • Heat-resistant handling tools

    Results and Deliverables

    • Ignition loss percentage (%)
    • Calculated resin content (if applicable)
    • Calculated fiber content (%)
    • Test report with specimen details
    • Quality control documentation

    Frequently Asked Questions

    ASTM D2584 is a test method used to determines resin, fiber, and filler content of cured reinforced plastics using ignition loss procedure.

    ASTM D2584 is primarily used for glass fiber reinforced thermoset composites such as polyester, vinyl ester, and epoxy resins where the matrix can be safely burned off.

    The standard recommends heating the specimen to approximately 565°C (1050°F) to ensure complete resin burn-off while preventing damage or degradation of the glass fiber reinforcement.

    The standard measures Barcol hardness, which indicates resistance to surface indentation and provides an indirect evaluation of stiffness and cure condition.

    It ensures correct glass fiber content, which directly influences strength, stiffness, durability, and structural performance of composite material.

    Case Studies

    In-depth examination of genuine material testing solutions

    Case Study: Dopant & Ultra-Low Concentration Analysis via…

    banner

    Case Study: Dopant & Ultra-Low Concentration Analysis via…

    Introduction to STEM-EELS for Elemental Analysis Scanning Transmission Electron Microscopy (STEM) combined with Electron Energy Loss...

    Read Case Study

    Analysis of PVC Pipe Degradation Using FTIR Spectroscopy

    Fourier Transform Infrared Spectroscopy (FTIR)

    Analysis of PVC Pipe Degradation Using FTIR Spectroscopy

    PVC Pipe in Infrastructure — and Why Degradation Matters Polyvinyl chloride (PVC) pressure pipe is one...

    Read Case Study

    Nano-scale roughness measurement of Si-wafers by Atomic Force…

    banner

    Nano-scale roughness measurement of Si-wafers by Atomic Force…

    Nano-scale surface roughness is a critical parameter in fabricated thin-films that are used in optics, solar...

    Read Case Study
     Request a Quote

    Request a Quote

    Submit your material details and receive testing procedures, pricing, and turnaround time within 24 hours.



    • ddd
      Quick Turnaround and Hasslefree process
    • ddd
      Confidentiality Guarantee
    • ddd
      Free, No-obligation Consultation
    • ddd
      100% Customer Satisfaction
    Home / ASTM / ASTM D2584 Ignition Loss of Cured Reinforced Resins

    Discover more from Infinita Lab

    Subscribe now to keep reading and get access to the full archive.

    Continue reading

    ×

    Talk to an Expert

      Connect Instantly

      (888) 878-3090
      Ensure Quality with the Widest Network of Accredited Labs
      • ddd
        Quick Turnaround and Hasslefree process
      • ddd
        Confidentiality Guarantee
      • ddd
        Free, No-obligation Consultation
      • ddd
        100% Customer Satisfaction

        ddd

        Start Material Testing