Introduction 

ASTM E384 describes a method for determining the microindentation hardness testing of materials, and it is mainly applied using either the Knoop or the Vickers hardness test procedures. These hardness test procedures have been commonly applied to small test specimens or regions of particular interest in the material, and they quantify material hardness at meager test forces. Material science and engineering applications use the techniques for testing hardness, a critical material property that commonly determines material performance.

Scope of ASTM E384

The ASTM E384 test method covers the determination of the microindentation hardness of materials using either the Vickers or Knoop indenter system. These methods apply to metallic and non-metallic materials as well as coatings. This is highly useful in determining the hardness of materials where it is impossible to do tests using conventional macro-hardness due to their very small, thin, or brittle nature.

ASTM E384 Test Procedure

The test equipment used in ASTM E384 are as follows:

ParticularsDetails
Intender Vickers indenter: The Vickers indenter is a diamond indenter in a square pyramid geometry where 136° exists between opposite faces.
Knoop indenter: An elongated diamond indenter creates impressions that are rhombohedral in shape. It is used in anisotropic materials and surfaces prone to cracking.
Hardness Testers Special microhardness testing machines provide very accurate application of force, usually from 1 gf to 1000 gf.
Further, the dimensions of the indentations are measured using an optical microscope since the resulting indentations are very small.

Test Preparation of ASTM E384

The surface being tested should be flat, smooth, clean, and contamination-free since this can influence the testing of hardness. The specified surface of a Vickers or Knoop indenter is pressed onto the material surface by a predetermined load. The applied load is then maintained for a prescribed dwell period of 10 to 15 seconds. Further, using a microscope, the resulting indentation is measured after indentation – its diagonals (Vickers) or long and short axes (Knoop). Also, the hardness value depends on the size of the indent.

Result Analysis

The calculation and result of ASTM E384 are as follows:

Calculation Report
The following data is calculated in ASTM E384:

The Knoop Hardness Number:
P = force
Ap = projected area of indentation

The Vickers Hardness Number:
Where,
P = force
As = surface area of the indentation.
The hardness number that results from a calculation based on the load applied and the indentation size is usually reported. The load was used during testing.
The diagonal length or dimensions of indentation
Any conditions of the test, such as dwell time and test temperature.

Specimen Size

Optimally, for ASTM E384, the test specimen should be flat with a polished surface free of preparation-induced damage. Furthermore, the surface must be free of any problems that could affect the indentation or the subsequent measurement of the diagonals. 

Applications of ASTM E384

Metallurgy: It connects metal hardness to its microstructure, making it an essential application in controlling the quality of materials and the selection process.

Aerospace: Determines the performance as well as reliability of components subjected to a high-stress environment, thus complying with safety standards.

Biomedical: It tests the hardness of biomaterials and coatings of implants to ensure compatibility with biological systems and durability.

Electronics: It evaluates the hardness of hard coatings and materials used in electronic components. Hence, it enhances their performance and life span.

Automotive: Determines the hardness levels of microstructures in components of engines and gears to resist wear effects.

Manufacturing: Helps develop quality advanced materials and coatings for various applications.

Conclusion

The ASTM E384 test method is significant, as it defines hardness for small, thin, or brittle materials.  On thin films, coatings, and minor components, this test permits the user to determine the hardness and, thereby, have an approximate indication of properties such as wear resistance, toughness, and material homogeneity. Further, using Vickers or Knoop indenters, very accurate hardness measurements are possible using low forces. It employs various applications in material characterization, quality control, and research.

FAQs

What are the fundamental differences between the Vickers and Knoop test methods?

The Vickers test method uses a square-pyramidal indenter that gives a more symmetrical indentation, whereas the Knoop test method uses an elongated rhombic indenter. The Knoop test method is preferred for tests on anisotropic materials or when testing brittle surfaces.

What are some of the applications of ASTM E384?

It sees wide applications in the testing of coatings, thin films, microstructures in metals and ceramics, and minor components, which are difficult to test by methods at the macro level.

What are typical forces used for micro indentation tests?

The forces usually range from 1 gf to 1000 gf, depending on the material and the depth to which indentation is to be made.

What does microhardness reveal about the material?

The concept of mechanical properties, such as material wear resistance, ductility, and strength, can be estimated by measuring microhardness. ASTM E384 test is helpful for the determination of surface treatments and coatings.

Does ASTM E384 standard test apply to nonmetals?

This test method, in principle, can be applied to most materials, such as different types of ceramics, polymers, composites, and metallic materials.


Talk to Our Experts Today!

Submit your contact info and we’ll get back to you within 24 hours

    Full Spectrum of ASTM Material Testing — Backed by 2,000+ Trusted Lab Partners

    Polymers and Plastics

    ASTM standards for chemical composition, physical properties, failure analysis, and other routine and non-routine testing for polymers and plastics

    See All Polymers and Plastics Test
    Ceramics

    ASTM standards for determination of mechanical, physical, and thermal properties, and performance of monolithic and composite ceramics

    See All Ceramics Test
    Metals and Alloys

    ASTM standards guiding various destructive, non-destructive and analytical tests for quality control of different metals and alloys

    See All Metals and Alloys Test
    Chemical Analysis

    ASTM standards for chemical analysis of solid, liquid and gaseous materials for specification compliance and quality control

    See All Chemical Analysis Test
    Paints and Coatings

    ASTM standards for various chemical, physical, stability and exposure analysis of paints and coatings

    See All Paints and Coatings Test

    Our Services

    Metrology

    Metrology

    A variety of microscopy and spectroscopy tools available for precise measurements from the nano to the meter scale.

    Learn More
    Materials Testing

    Materials Testing

    ASTM and ISO standard and custom chemical, mechanical, thermal, corrosion tests, etc. for all materials metals, ceramic or polymers.

    Learn More
    Product Testing

    Product Testing

    Thousands of tests for product quality and reliability under heat, humidity, temperature shock, vibration, drop, electrostatic discharge.

    Learn More
    Home / ASTM / ASTM E384 Test for Microindentation Hardness of Materials

    Discover more from Infinita Lab

    Subscribe now to keep reading and get access to the full archive.

    Continue reading

    ×

    Talk to an Expert

      Connect Instantly

      (888) 878-3090
      Ensure Quality with the Widest Network of Accredited Labs
      • ddd
        Quick Turnaround and Hasslefree process
      • ddd
        Confidentiality Guarantee
      • ddd
        Free, No-obligation Consultation
      • ddd
        100% Customer Satisfaction

        ddd

        Start Material Testing