Introduction

This ASTM standard, E928, describes a test method that employs differential scanning calorimetry and the Van’t Hoff equation to determine the purity of materials with more than 98.5 mole % purity. Moreover, it is one of the new methods for purity assessment based on the melting behavior of materials and the released heat flow.

Scope of ASTM E928

The technique estimates the purity of organic chemicals by measuring their melting points and the amount of heat accompanying the melting process. The purity can be judged from the melting range and melting enthalpy from the DSC analysis. The broader the melting temperature range, the higher the increase in the impurity level of a compound. This phenomenon is described approximately by the Van’t Hoff equation for melting point depressions. Furthermore, the ASTM E928 test is utilized in quality control, specification acceptance, and research. 

Test Procedure of ASTM E928

Principle of DSC:

The Differential Scanning Calorimetry (DSC) technique involves heating a small sample of the material at a controlled rate. As the material melts, it absorbs heat, resulting in an endothermic peak on the DSC curve. The shape and area of this peak provide information about the melting behavior and purity of the substance. The heat flow into the sample is compared to a reference material, and the difference in heat flow (differential) is recorded.

The ASTM E928 test procedure and other details are as follows:

ParticularsDetails
Sample PreparationA few milligrams of organic chemicals are placed into a DSC pan. 
HeatingHeating at a controlled rate (1 to 10°C/min) until melting occurs. The temperatures at which melting begins and when the sample is entirely melted are recorded
Data AnalysisThe DSC curve of heat flow versus temperature was analyzed using the onset of melting, peak melting temperature, and heat of fusion. 
The area underneath the melting peak corresponds to the heat of fusion, which generally relates to sample purity.
Result Van’t Hoff Equation: This equation connects the depression of the melting point with the sample’s purity. The heat of fusion, in addition to an observed melting range, is considered in this equation.
Purity Calculation: The purity of the sample is determined through the melting point depression, that is, the difference between the melting point of the pure substance and the observed melting point.

Specimen Size of ASTM E928

  • The test sample (liquid or solid) should be mixed before sampling and sampled by removing portions from various parts of the container.
  • The portions should be mixed well to provide a representative sample for the purity determinations.
  • Only 1 to 3 mg is required for each analysis. Also, any physical or mechanical treatment of the material should be avoided that will cause chemical changes.

Applications

  • Organic Chemicals: Purity assessment for research and manufacturing.
  • Assuring Quality: This technique is used in quality control laboratories to determine if a substance contains impurities.

Conclusion:

ASTM E928 employs a technique similar to DSC for assessing the purity of organic chemicals based on their melting behavior. This test relies on the melting point depression relationship, which can be directly related to purity with high accuracy and efficiency. Furthermore, this standard has widespread application in industries where the purity of the organic compound is of prime importance, such as pharmaceuticals or chemical manufacturing.

Infinita Lab offers comprehensive ASTM D928 testing services, a Comprehensive lab network, project management, confidentiality, and rapid turnaround. Trust Infinita Lab for your material testing needs, Faster test results, cost savings, and reduced administrative workload.

Looking for a trusted partner to achieve your research goals? Schedule a meeting with us, send us a request, or call us at (888) 878-3090 to learn more about our services and how we can support you. Request a Quote

FAQs

What is ASTM E928?

ASTM E928 outlines procedures for determining sound power levels in various environments, ensuring that results are consistent and reliable.

What are the advantages of Purity determination?

The DSC is an accurate and dependable method for purity determination. Only a few samples are needed, and the test can be done in a relatively shorter time.

Why is ASTM E928 important for determining purity?

ASTM E928 provides one accurate, reliable method for determining organic chemical purity. Purity is a critical issue in many industries, as pharmaceutical impurities can affect a product's safety and efficacy.

How long does it take to perform a purity test using ASTM E928?

Depending on the heating rate and the complexity of the analysis, the test can be completed relatively quickly, often within a few hours.

What are the limitations of ASTM E928?

ASTM E928 is an excellent method for assessing the purity of organic compounds; it may not be appropriate for substances with extremely complicated melting behaviors or materials with poorly defined melting points.


3 Easy Steps
to Start Testing

  • Share Your Testing Material Details with Us
  • Hassle-Free Collection Pick-Up Service
  • We Find the Lab, You Get the Results
Arrow

Error: Contact form not found.

Case Studies

In-depth examination of genuine material testing solutions

Case Study: Dopant & Ultra-Low Concentration Analysis via…

Infinita Engineering Visual showing Case Study Dopant microscopy / imaging workflow for case study: dopant & ultra-low concentration analysis via stem-eels.

Case Study: Dopant & Ultra-Low Concentration Analysis via…

Introduction to STEM-EELS for Elemental Analysis Scanning Transmission Electron Microscopy (STEM) combined with Electron Energy Loss...

Read Case Study

AFM Nano-Scale Roughness Measurement Guide for Silicon Wafers

Infinita Engineering Visual showing Afm Nano Scale general testing / industry guide workflow for afm nano-scale roughness measurement guide for silicon wafers.

AFM Nano-Scale Roughness Measurement Guide for Silicon Wafers

Nano-scale surface roughness is a critical parameter in fabricated thin-films that are used in optics, solar...

Read Case Study

Talk to Our Experts Today!

Submit your contact info and we’ll get back to you within 24 hours

    Home / services / ASTM E928: Purity By DSC Testing Services

    Discover more from Infinita Lab

    Subscribe now to keep reading and get access to the full archive.

    Continue reading

    ×

    Talk to an Expert

      Connect Instantly

      (888) 878-3090
      Ensure Quality with the Widest Network of Accredited Labs
      • ddd
        Quick Turnaround and Hasslefree process
      • ddd
        Confidentiality Guarantee
      • ddd
        Free, No-obligation Consultation
      • ddd
        100% Customer Satisfaction

        ddd

        Start Material Testing