ToF-SIMS Surface Chemical Analysis Testing
Time-of-Flight Secondary Ion Mass Spectrometry (TOF-SIMS) generates secondary ions from the surface of a sample by bombardment with a beam of high energy primary ions. The resulting secondary ions of various analyte species are then identified by Time of Flight Mass spectrometry. Surface composition as well as near surface depth profiles can be obtained.

TRUSTED BY




Precision-driven testing for dimensional accuracy and compliance
- Overview
- Test Process
- Specifications
- Instrumentation
- Results and Deliverables
Overview
Time of Flight Secondary Ion Mass Spectrometry (TOF-SIMS) is an advanced surface analysis technique that is utilized to identify the chemical composition of materials at very small scales. TOF-SIMS is based on bombarding the surface of a sample with a focused ion beam, from where secondary ions are emitted.
These ions are recognized on the basis of their time of flight in a mass spectrometer. TOF-SIMS is an important tool for analyzing thin films, semiconductors, polymers, biomaterials, and contaminants owing to its very high surface sensitivity.

Scope
TOF-SIMS testing evaluates the chemical composition and molecular distribution of material surfaces and thin layers. The technique enables highly sensitive detection of elements and compounds present on the outermost surface of materials.
The scope includes:
Surface chemical composition analysis
Detection of trace contaminants and impurities
Elemental and molecular identification
Thin film and coating characterization
Depth profiling of layered materials
Applications
Semiconductor and microelectronics analysis
Polymer and coating characterization
Thin film and multilayer material analysis
Biomedical and biomaterial research
Surface contamination and failure analysis
Benefits
Extremely high surface sensitivity (ppm–ppb level)
Provides elemental and molecular information
Enables surface imaging and chemical mapping
Supports depth profiling of multilayer structures
Useful for failure analysis and quality control
Test Process
Sample Preparation
The sample surface is cleaned and mounted in the vacuum chamber to ensure accurate surface analysis.
1Primary Ion Bombardment
A focused primary ion beam strikes the sample surface, ejecting secondary ions from the outermost layers.
2Time-of-Flight Mass Analysis
The emitted ions travel through a time-of-flight analyzer, where their mass-to-charge ratio is determined.
3Data Processing and Interpretation
The detected ions are analyzed to generate mass spectra and maps that reveal surface composition.
4Technical Specifications
| Parameter | Details |
|---|---|
| Technique Type | Surface chemical analysis |
| Ion Source | Primary ion beam |
| Mass Analyzer | Time-of-Flight mass spectrometer |
| Analysis Depth | ~1–2 nm surface layer |
| Detection Sensitivity | Parts per million (ppm) to parts per billion (ppb) |
| Spatial Resolution | Up to sub-micrometer level |
| Operating Environment | Ultra-high vacuum (UHV) |
| Data Output | Mass spectra, chemical images, depth profiles |
Instrumentation Used for Testing
TOF-SIMS Analyzer
Primary Ion Source
Ultra-High Vacuum Chamber
Ion Detector System
Data Acquisition and Analysis Software
Results and Deliverables
Surface chemical composition report
Mass spectra analysis
Elemental and molecular identification
Surface chemical imaging maps
Depth profile analysis report
Frequently Asked Questions
TOF-SIMS is an advanced surface analysis technique that uses ion bombardment and mass spectrometry to identify elements, isotopes, and molecular fragments on material surfaces with extremely high sensitivity and spatial resolution.
TOF-SIMS provides detailed information about surface chemical composition, molecular fragments, elemental distribution, and trace contaminants. It can also generate chemical maps and depth profiles of thin films or layered structures.
TOF-SIMS typically analyzes the outermost 1–2 nanometers of the material surface. With controlled sputtering, it can also perform depth profiling to study multilayer structures and thin film interfaces.
TOF-SIMS is important in semiconductor manufacturing because it can detect extremely small amounts of impurities, dopants, and contaminants that may affect device performance, reliability, and manufacturing quality.
Unlike conventional mass spectrometry, TOF-SIMS focuses on analyzing the outermost surface layers of materials using ion bombardment, enabling detailed chemical mapping and surface-sensitive analysis at microscopic scales.
Why Choose Infinita Lab for Advanced Materials Testing and Characterization?
At the core of this breadth is our network of 2,000+ accredited laboratories across the USA, offering access to over 10,000 testing methods and analytical services. From advanced materials characterization (SEM, TEM, RBS, XPS) to mechanical, chemical, environmental, biological, and standardized ASTM/ISO-compliant testing, we deliver unmatched flexibility, specialization, and scale. You are never limited by geography, facility, or methodology — Infinita Lab connects you to the right expertise and testing solution, every time.
Looking for a Trusted Partner for Accurate and Reliable Testing Services?
Send query us at hello@infinitlab.com or call us at (888) 878-3090 to learn more about our services and how we can support you.

Request a Quote
Submit your material details and receive testing procedures, pricing, and turnaround time within 24 hours.
Quick Turnaround and Hasslefree process

Confidentiality Guarantee

Free, No-obligation Consultation

100% Customer Satisfaction