    Overview

    ASTM G46 is used to examine and evaluate pitting corrosion in metallic materials. The test provides methods for identifying, measuring, and characterizing pits formed on metal surfaces due to localized corrosion.

    This method is widely applied in corrosion studies, failure analysis, and material performance evaluation. It helps engineers assess the severity of pitting, understand corrosion mechanisms, and determine the suitability of materials for corrosive environments.

    Scope

    ASTM G46 evaluates pitting corrosion by providing procedures to measure pit depth, density, and distribution on metal surfaces. The test enables quantitative and qualitative assessment of localized corrosion damage.

    ASTM G46 evaluates:

    • Depth of corrosion pits on metal surfaces
    • Density and distribution of pits
    • Severity of localized corrosion damage
    • Surface condition after corrosion exposure
    • Corrosion behavior of metallic materials

    Applications

    • Corrosion testing of metals and alloys
    • Oil and gas industry components
    • Marine and offshore structures
    • Chemical processing equipment
    • Aerospace and automotive materials
    • Failure analysis and material evaluation

    Benefits

    • Provides a standardized evaluation of pitting corrosion
    • Helps assess the severity of localized corrosion damage
    • Supports material selection for corrosive environments
    • Assists in failure analysis and root cause investigation
    • Enables comparison of corrosion resistance between materials

    Test Process

    Sample Preparation

    Corroded specimens are cleaned to remove corrosion products without altering pit geometry.

    1

    Surface Examination

    The surface is visually and microscopically examined to identify pits.

    2

    Pit Measurement

    Pit depth, size, and distribution are measured using appropriate techniques.

    3

    Data Recording & Evaluation

    The measured data is analyzed to assess pitting severity and corrosion behavior.

    4

    Technical Specifications

    ParameterDetails
    Applicable MaterialsMetals and alloys
    Pit Depth Range~1 µm to 5 mm
    Pit Diameter Range~10 µm to 10 mm
    Measurement ResolutionUp to 0.1 µm (microscopy/profilometry)
    Magnification Range10× to 500×
    Evaluation CriteriaPit depth, density (pits/cm²), and distribution

    Instrumentation Used for Testing

    • Optical microscope (10×–500×)
    • Surface profilometer (resolution up to 0.1 µm)
    • Measuring microscope or depth gauge
    • Sample cleaning equipment (chemical/ultrasonic)
    • Image analysis software
    • Data acquisition system

    Results and Deliverables

    • Pit depth and diameter measurements
    • Pit density (pits/cm²) data
    • Corrosion severity classification
    • Surface morphology analysis
    • Test condition summary
    • ASTM compliance report

    Frequently Asked Questions

    ASTM G46 includes pit depth measurement, pit density, pit distribution, surface area affected, and metallographic examination, evaluating severity of pitting corrosion and providing quantitative and qualitative assessment of localized corrosion damage.

    ASTM G46 uses visual inspection, optical microscopy, profilometry, and metallographic techniques to measure pit characteristics and assess corrosion damage on metal surfaces.

    ASTM G46 is commonly applied to metals and alloys such as stainless steels, aluminum alloys, and other corrosion-resistant materials exposed to aggressive environments.

    ASTM G46 evaluates pit size, depth, density, and distribution, providing data to assess corrosion severity and predict potential impact on structural integrity.

    ASTM G46 evaluates pitting corrosion after exposure and does not predict initiation mechanisms, requiring additional testing to understand environmental factors and long-term corrosion behavior.

    Why Choose Infinita Lab for Advanced Materials Testing and Characterization?

    At the core of this breadth is our network of 2,000+ accredited laboratories across the USA, offering access to over 10,000 testing methods and analytical services. From advanced materials characterization (SEM, TEM, RBS, XPS) to mechanical, chemical, environmental, biological, and standardized ASTM/ISO-compliant testing, we deliver unmatched flexibility, specialization, and scale. You are never limited by geography, facility, or methodology — Infinita Lab connects you to the right expertise and testing solution, every time.

    brain

    Looking for a Trusted Partner for Accurate and Reliable Testing Services?

    Send query us at hello@infinitlab.com or call us at (888) 878-3090 to learn more about our services and how we can support you.

     Request a Quote

    Request a Quote

    Submit your material details and receive testing procedures, pricing, and turnaround time within 24 hours.



    • ddd
      Quick Turnaround and Hasslefree process
    • ddd
      Confidentiality Guarantee
    • ddd
      Free, No-obligation Consultation
    • ddd
      100% Customer Satisfaction
    Home / Materials, Metrology & Product Testing Services / ASTM G46 Pitting Corrosion Examination & Evaluation Testing

    Discover more from Infinita Lab

    Subscribe now to keep reading and get access to the full archive.

    Continue reading

    ×

    Talk to an Expert

      Connect Instantly

      (888) 878-3090
      Ensure Quality with the Widest Network of Accredited Labs
      • ddd
        Quick Turnaround and Hasslefree process
      • ddd
        Confidentiality Guarantee
      • ddd
        Free, No-obligation Consultation
      • ddd
        100% Customer Satisfaction

        ddd

        Start Material Testing